Galvanized Steel Wire Rope Overall Operation Process
May 27, 2017

Galvanized steel wire rope overall operation process is still very complex, if any one of the details of the problem, then the products produced by the clearance. Heat treatment is also one of the operational aspects, and how do we heat it work?

First of all, before we heat the raw materials of the product should be checked before the use of some of the materials used is not in line with the use of standards, heat treatment to use the disk surface can not be cracked and more serious scratches, if the above has folded and ears And other issues can not be put into use.

Second, after the heat treatment of galvanized steel wire rope semi-finished products, but also need to meet the technical requirements of manufacturers acceptance. The surface of the semi-finished product can not have serious corrosion problems, and can not have any bruises and scratches.

If the product above the oil and other problems such as defects, then we can not put into use. And if it is finished steel products, and is the use of quenching for processing, and can only ride a slight wind rust.

Drawing is galvanized steel wire rope production process will experience an operation link, and in the staff drawing when the need to pay attention to what kind of problem?

When we work with our staff, try to keep the water flow between the inside of the drum and the mold box, and if the wire has been cooled and the water is broken, the operation of the vehicle should be stopped. Under normal circumstances, the mold box temperature temperature can not be more than 50 degrees Celsius, and the tank inside the lubricating fluid is also need to maintain the cycle of the state, the temperature of the lubricant can not exceed 75 degrees Celsius, each shift need to conduct a check.

When we are drawing, we should pay attention to the strict compliance with the order of operation. It is not possible to operate in a way of a jump mold. The diameter of the wire on the wire rope should also be carefully checked and can be retained within the permissible deviation. But if its diameter has exceeded the specified range of errors, it should be replaced in a timely manner, can not continue to put into the next operating line.